Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.63 J/cm² | 7.76 ft-lb/in² | |
Eastman Tenite 130-33 Cellulose Acetate
(discontinued **) 33% Plasticized, contains 100% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 1.63 J/cm² | 7.76 ft-lb/in² | |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |