Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
ISO 179/1eA
Radici Radilon® AERV1906 LK (dry) Nylon 66
Glass-fiber reinforced with high impact strength, heat stabilizedInformation provided by Radici group.
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 HS-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced
Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
ISO 179/1eA
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin
Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri..
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
DIN 53453
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene
CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI..
Charpy Impact, Notched 1.15 J/cm²

@Temperature 23.0 °C
5.47 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnite® TV4 290 PBT-GF50
50% Glass Reinforced
Charpy Impact, Notched 1.15 J/cm²

@Temperature 30.0 °C
5.47 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi..
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
ISO 179
BASF Petra® 140 45% Glass Filled PET
Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex..
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
ISO 179
BASF Petra® 140 BK-112 45% Glass Filled PET
Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa..
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Conditioned)
Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold...
Charpy Impact, Notched 1.15 J/cm²

@Temperature -30.0 °C
5.47 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
Conditioned; ISO 179/IeA
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.
Copyright © lookpolymers.com All Rights Reserved