Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.05 J/cm² @Temperature 22.8 °C |
5.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Charpy Impact, Notched | 1.05 J/cm² @Temperature 22.8 °C |
5.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | ISO 179/1eA |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Charpy Impact, Notched | 1.05 J/cm² @Temperature -30.0 °C |
5.00 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 371A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Charpy Impact, Notched | 1.05 J/cm² @Temperature -30.0 °C |
5.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | |
Arkema Group Orgalloy® RS 6020 Nylon 6 Alloy, 20% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties... |
|||
Charpy Impact, Notched | 1.05 J/cm² @Temperature -30.0 °C |
5.00 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MB 3750 Nylon 11, Transparent Grade (Dry) Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical.. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced PEEKInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 1.05 J/cm² | 5.00 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBATER BFA30 PBT, 30% glass fiber reinforced, flame retardant PBT-GF30 FRInformation provided by BARLOG plastics GmbH. |