Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® plus + FP Polyethylene Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “.. |
|||
Charpy Impact, Notched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | |
LATI Latamid 6 E02 PA 6, Impact modified Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A... |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179/1EA-1993 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 246M PA66, Conditioned Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO Data |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO Data |
Dow Prevail® 3100 ABS + Polyurethane PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Charpy Impact, Notched | 10.0 J/cm² @Temperature -20.0 °C |
47.6 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene Applications which require high wear resistance - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Braskem. |
|||
Charpy Impact, Notched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 5041 Ultra High Molecular Weight Polyethylene Applications which require high wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Bras.. |
|||
Charpy Impact, Notched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided by Braskem. |
|||
Charpy Impact, Notched | >= 10.0 J/cm² | >= 47.6 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 6541 Ultra High Molecular Weight Polyethylene Applications which require highest wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided b.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179 |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |
|||
Charpy Impact, Notched | 10.0 J/cm² | 47.6 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |