Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179/1eU |
Total Lacqrene® 3351(EU) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.05 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 358-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene GM2860 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179/1eA |
Styron CALIBREâ„¢ 7100-15 Polycarbonate CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179/1eA |
Styron CALIBREâ„¢ 7101-15 Polycarbonate CALIBREâ„¢ 7101-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179/1eA |
Styron CALIBREâ„¢ 7102-15 Polycarbonate CALIBREâ„¢ 7102-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179/1eA |
Styron CALIBREâ„¢ 7103-15 Polycarbonate CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | IS0179 |
Zhejiang Juner 301-G25 25% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | IS0179 |
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179/1eA |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -20.0 °C |
4.05 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO 179 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.05 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 0.850 J/cm² | 4.05 ft-lb/in² | |
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good.. |
|||
Charpy Impact, Notched | 0.850 - 1.60 J/cm² | 4.05 - 7.61 ft-lb/in² | Average value: 1.06 J/cm² Grade Count:14 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.05 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 179/1eA |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |