Polymer Property : Charpy Impact, Notched = 37.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer
18 MFR LEXAN High Flow Ductile Copolymer
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East)
18 MFR LEXAN High Flow Ductile Copolymer
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific)
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East)
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific)
18 MFR LEXAN High Flow Ductile Copolymer
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
ISO Data
Styron Pulse® 710 ABS + Polycarbonate
PULSE® 710 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 710 Engineering resin h..
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
ISO 179
BASF Ultramid® B3Z BK 30464 PA6 (Dry)
Description: Ultramid B3Z BK30464 is an impact-modified, pigmented black, unreinforced PA6 for injection molding.Applications: Impact-resistant articles, e.g. dowels.Information provided by BASF
Charpy Impact, Notched 7.90 J/cm²
37.6 ft-lb/in²
ISO 179/1eA
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..