Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.70 J/cm² | 36.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7664 PC Copolymer (Asia Pacific) Lexan* ML7664 polycarbonate (PC) siloxane resin, is a product targeting (profile) extrusion applications requiring extreme low temperature ductility. Lexan* ML7664 resin is a non-FR product availabl.. |
|||
Charpy Impact, Notched | 7.70 J/cm² | 36.6 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |