Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:.. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179 |
GEHR Plastics PEEK Polyetheretherketone Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical re.. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment... |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Connector AS PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 0.820 J/cm² @Temperature -30.0 °C |
3.90 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Charpy Impact, Notched | 0.820 J/cm² @Temperature -30.0 °C |
3.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | |
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers. |
|||
Charpy Impact, Notched | 0.820 J/cm² | 3.90 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |