Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Charpy Impact, Notched | 0.650 - 10.0 J/cm² | 3.09 - 47.6 ft-lb/in² | Average value: 2.30 J/cm² Grade Count:43 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.650 - 10.0 J/cm² | 3.09 - 47.6 ft-lb/in² | Average value: 4.80 J/cm² Grade Count:50 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2300LC Polypropylene Block Copolymer CHARACTERISTICS: HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR FURNITURES, HOUSEWARES, CLOSURES, CONTAINERS, CRATES, AUTOPARTS AND ELECTRICAL APPLIANCES |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST35G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | |
LATI Latilub 57-30GRTS G/20 PPA, 20% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | |
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET) 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information .. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced PEEK-CF30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | DIN 53453 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 1791/eU |
Total Lacqrene® 851 High Impact Polystyrene
(discontinued **) LACQRENE® 851 is a flame retardant, high impact polystyrene, halogen free rated UL 94 V0 @ 2.5 mm and UL 94 5VA @ 2mm. LACQRENE® 851 offers rheological and mechanics properties which permits larg.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Radici Heraform® R 900 Acetal Copolymer Standard grade for injection molding of details with high mechanical requirement.Information provided by Radici group. |