Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Asia Pacific) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combines |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Asia Pacific) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 1173X PC Copolymer (Europe-Africa-Middle East) Lexan* 1173X polycarbonate (PC) resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-30 C) ductility in combination with high flow characteristics an.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East) LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Asia Pacific) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® ML3042 PC (Europe-Africa-Middle East) LEXAN ML3042 offers an extremely low light transparency in combination with a very high reflection. This product is ideally suited for lighting reflectors. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EX1632T PC (Europe-Africa-Middle East) LEXAN* EX1632T polycarbonate resin, MVR (300C/1.2kg) 6 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179 |
Manifattura Cattaneo PP H Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | |
LATI Latistat 63-08 PA6, Impact Modified Dissipative product based on Polyamide 6 (PA6), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/1eA |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/1eA |
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal.. |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1 |
Total HDPE 56020 S High Density Polyethylene - Blow Molding HDPE 56020 S is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack Resi.. |
|||
Charpy Impact, Notched | 5.00 - 10.0 J/cm² | 23.8 - 47.6 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | double V-notch, rk=1.5 mm; DIN 53753 |
Zell-Metall Engineering Plastics Zellamid 250 GF 30 (PA6.6 + 30% glass fiber) Zellamid® 250 GF 30 (PA 6.6 + 30% Glassfibre, black) is the registered trademark for Zell-Metalls 30% glass fiber reinforced nylon grade 6.6. It offers increased strength, stiffness, creep res.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner JEPP2056 PP For Automotive Parts Applications: BumpersInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4188 nat PA612 Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosi.. |
|||
Charpy Impact, Notched | >= 5.00 J/cm² | >= 23.8 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem Idealis 500 High Molecular Weight Polyethylene Powder Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards a.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179-1 |
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)... |
|||
Charpy Impact, Notched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Charpy Impact, Notched | 5.00 J/cm² | 23.8 ft-lb/in² | |
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced Polyurethane (PUR) based compound. Glass fibers. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |