Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.610 J/cm² @Temperature -30.0 °C |
2.90 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 0.610 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
2.90 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.17 J/cm² Grade Count:30 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | ISO 179/1eA |
Polyplastics FR-PET® BN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | ISO 179/1eA |
Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.609 J/cm² @Temperature 22.8 °C |
2.90 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMU 308 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed with good stiffness/toughness balance fro electrical appliance such as washing machine and dryer stands.Availability: Africa .. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent... |
|||
Charpy Impact, Notched | 0.610 J/cm² @Temperature -30.0 °C |
2.90 ft-lb/in² @Temperature -22.0 °F |
ISO data |
BASF Capron® HPN 9315G Impact Modified, 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9315G is a 15% glass reinforced, impact modified polyamide 6 injection molding grade resin in the High Productivity Nylon Series developed for applications requiring superior dry-as-molde.. |
|||
Charpy Impact, Notched | 0.610 J/cm² @Temperature -20.0 °C |
2.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | ASTM D256 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Charpy Impact, Notched | 0.610 J/cm² | 2.90 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |