Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 45FS GF20 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
Radici Radilon® CS38 Copolyamide 6 semiaromatic Film extrusion gradeInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179 |
Nilit Polynil® P50FI Internally Lubricated Nylon 66 Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long.. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | DIN 53453 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 7760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7760 is a heterophasic copolymer. PPC 7760 is characterized by medium fluidity offering a combination of ease of processing and excellent impact properties in applications ranging.. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 30.0 °C |
2.86 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® EBV-2H PA6-GF20 Product description: Grilon EBV-2H is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 20% glass fibers. Grilon EBV-2H has the following important properties: High melt streng.. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 30.0 °C |
2.86 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 30.0 °C |
2.86 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SK692FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179 / 1eA |
Asahi Kasei Tenac® 7054 Homopolymer Acetal Resin High-flow grade with high crystallization rate for higher productivity.Information provided by Asahi Kasei Corporation. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
Radici Heraform® R 3000 Acetal Copolymer Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROMID 6.6 Polyamide 6.6 This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL.. |
|||
Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |