Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.570 J/cm² @Temperature -20.0 °C |
2.71 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance.. |
|||
Charpy Impact, Notched | 0.570 J/cm² | 2.71 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Charpy Impact, Notched | 0.570 J/cm² | 2.71 ft-lb/in² | ISO 179 |
BASF Ultramid® NBX-0025 NF2001 PA66 (Dry) Ultramid NBX-0025 NF2001 is a specialty, unfilled PA6/6. |
|||
Charpy Impact, Notched | 0.570 J/cm² | 2.71 ft-lb/in² | ISO 179 |
BASF Ultramid® 1000-11 NF2001 PA66 (Dry) Ultramid 1000-11 NF2001 is a general purpose nylon 6/6. |
|||
Charpy Impact, Notched | 0.570 J/cm² | 2.71 ft-lb/in² | ISO 179 |
BASF Ultramid® 1000-2 NF2001 PA66 (Dry) Ultramid 1000-2 NF2001 is a general purpose PA6/6. |
|||
Charpy Impact, Notched | 0.570 J/cm² | 2.71 ft-lb/in² | ISO 179 |
BASF Ultramid® 1003-2 NF2002 PA66 (Dry) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |