Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.340 J/cm² @Temperature -30.0 °C |
1.62 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 371A-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 0.340 - 0.500 J/cm² | 1.62 - 2.38 ft-lb/in² | Average value: 0.413 J/cm² Grade Count:3 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature -23.0 °C |
1.62 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-3300-RC Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-thin-walled parts, audio tapes, cupsInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179 |
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0 Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Prope.. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a.. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ASTM D256 |
Plenco 6582 Phenolic, Briquette, Injection Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Standard DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 2002U Polybutylene Terephthalate (PBT), Weather resistance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179-1 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature -30.0 °C |
1.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® S650FR BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced black flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Perfor.. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T357 Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.340 - 1.05 J/cm² @Temperature -30.0 - -30.0 °C |
1.62 - 5.00 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.707 J/cm² Grade Count:8 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Charpy Impact, Notched | 0.340 - 1.20 J/cm² | 1.62 - 5.71 ft-lb/in² | Average value: 0.851 J/cm² Grade Count:14 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Charpy Impact, Notched | 0.340 J/cm² | 1.62 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |