Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.310 - 1.30 J/cm² @Temperature -30.0 - 30.0 °C |
1.48 - 6.19 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.05 J/cm² Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Charpy Impact, Notched | 0.310 - 0.370 J/cm² @Temperature -30.0 - -30.0 °C |
1.48 - 1.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.340 J/cm² Grade Count:2 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Charpy Impact, Notched | 0.310 J/cm² @Temperature -30.0 °C |
1.48 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Charpy Impact, Notched | 0.310 J/cm² @Temperature -30.0 °C |
1.48 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.310 J/cm² | 1.48 ft-lb/in² | ASTM D256 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Charpy Impact, Notched | 0.310 J/cm² | 1.48 ft-lb/in² | ASTM D256 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Charpy Impact, Notched | 0.310 J/cm² @Temperature -40.0 °C |
1.48 ft-lb/in² @Temperature -40.0 °F |
Method B; Brittle Failure |
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6 30% crystallinity. Information supplied by Elastomer Engineering. |
|||
Charpy Impact, Notched | 0.310 J/cm² | 1.48 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 601SA Polybutylene Terephthalate (PBT), Low density, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.310 J/cm² | 1.48 ft-lb/in² | ASTM D256 |
Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Charpy Impact, Notched | 0.310 J/cm² | 1.48 ft-lb/in² | ASTM D256 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |