Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.205 - 0.251 J/cm² | 0.976 - 1.19 ft-lb/in² | Average value: 0.222 J/cm² Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.205 J/cm² | 0.976 ft-lb/in² | ASTM D256 |
Plenco 4527 Phenolic, Granular, Injection Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |