Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.203 J/cm² | 0.966 ft-lb/in² | ASTM D256 |
Plenco 4414 Phenolic, Granular, Injection Molded PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional .. |