Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.180 J/cm² @Temperature -40.0 °C |
0.857 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.180 - 0.220 J/cm² | 0.857 - 1.05 ft-lb/in² | Injection and Compression; ISO 179/1eA |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Charpy Impact, Notched | 0.180 J/cm² - NB @Temperature -30.0 - -20.0 °C |
0.857 ft-lb/in² - NB @Temperature -22.0 - -4.00 °F |
Average value: 0.640 J/cm² Grade Count:28 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ISO 179 |
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc. |
|||
Charpy Impact, Notched | 0.180 J/cm² @Temperature -30.0 °C |
0.857 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® 821 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection .. |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® Frost 902 70 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | |
LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ASTM D256 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ISO 179/1eA |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Charpy Impact, Notched | 0.180 J/cm² @Temperature 23.0 °C |
0.857 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Charpy Impact, Notched | 0.180 J/cm² @Temperature -30.0 °C |
0.857 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3200 H Polypropylene Blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.180 J/cm² @Temperature -30.0 °C |
0.857 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® EB-10 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.180 J/cm² @Temperature 23.0 °C |
0.857 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Charpy Impact, Notched | 0.180 J/cm² | 0.857 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® Frost 902 80 Acrylic Polymer Information provided by Lucite International |