Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.00 - 4.60 J/cm² @Temperature -30.0 - 30.0 °C |
4.76 - 21.9 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.45 J/cm² Grade Count:14 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |