Polymer Property : Charpy Impact, Notched = 22.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 12.0 - 22.0 J/cm²
57.1 - 105 ft-lb/in²
DIN 53453
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..