Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.60 - 2.60 J/cm² | 7.61 - 12.4 ft-lb/in² | Average value: 2.00 J/cm² Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Charpy Impact, Notched | 0.200 - 2.60 J/cm² @Temperature -20.0 - -20.0 °C |
0.952 - 12.4 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.39 J/cm² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.200 - 2.60 J/cm² @Thickness 102 - 102 mm |
0.952 - 12.4 ft-lb/in² @Thickness 4.00 - 4.00 in |
Average value: 1.39 J/cm² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |