Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 - 2.40 J/cm² | 0.714 - 11.4 ft-lb/in² | Average value: 1.20 J/cm² Grade Count:40 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact, Notched | 0.300 - 2.40 J/cm² | 1.43 - 11.4 ft-lb/in² | Average value: 0.904 J/cm² Grade Count:112 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |