Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.230 - 2.00 J/cm² | 1.09 - 9.52 ft-lb/in² | Average value: 0.820 J/cm² Grade Count:50 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact, Notched | 0.170 - 2.00 J/cm² | 0.809 - 9.52 ft-lb/in² | Average value: 0.756 J/cm² Grade Count:123 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Charpy Impact, Notched | 0.100 - 2.00 J/cm² | 0.476 - 9.52 ft-lb/in² | Average value: 1.00 J/cm² Grade Count:4 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.550 - 2.00 J/cm² @Temperature -30.0 - -30.0 °C |
2.62 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.974 J/cm² Grade Count:34 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.140 - 2.00 J/cm² | 0.666 - 9.52 ft-lb/in² | Average value: 0.508 J/cm² Grade Count:38 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.610 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
2.90 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.17 J/cm² Grade Count:30 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.200 - 2.00 J/cm² | 0.952 - 9.52 ft-lb/in² | Average value: 0.650 J/cm² Grade Count:7 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Charpy Impact, Notched | 0.400 - 2.00 J/cm² | 1.90 - 9.52 ft-lb/in² | Average value: 1.42 J/cm² Grade Count:24 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.600 - 2.00 J/cm² @Temperature -30.0 - 30.0 °C |
2.86 - 9.52 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.996 J/cm² Grade Count:13 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Charpy Impact, Notched | 1.00 - 2.00 J/cm² @Temperature -30.0 - 30.0 °C |
4.76 - 9.52 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.52 J/cm² Grade Count:20 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact, Notched | 0.150 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.714 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.863 J/cm² Grade Count:43 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact, Notched | 2.00 - 2.00 J/cm² @Temperature -30.0 - -30.0 °C |
9.52 - 9.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.00 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact, Notched | 0.100 - 2.00 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.596 J/cm² Grade Count:39 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Charpy Impact, Notched | 0.0300 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.143 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.413 J/cm² Grade Count:58 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |