Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 - 12.0 J/cm² | 2.38 - 57.1 ft-lb/in² | Average value: 2.36 J/cm² Grade Count:18 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 6.00 - 12.0 J/cm² | 28.6 - 57.1 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Charpy Impact, Notched | 0.100 - 12.0 J/cm² @Temperature -30.0 - 0.000 °C |
0.476 - 57.1 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 1.91 J/cm² Grade Count:27 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 3.00 - 12.0 J/cm² @Temperature -20.0 - 0.000 °C |
14.3 - 57.1 ft-lb/in² @Temperature -4.00 - 32.0 °F |
Average value: 7.67 J/cm² Grade Count:2 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.350 - 12.0 J/cm² @Temperature -23.0 - 0.000 °C |
1.67 - 57.1 ft-lb/in² @Temperature -9.40 - 32.0 °F |
Average value: 5.20 J/cm² Grade Count:3 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact, Notched | 0.100 - 12.0 J/cm² @Temperature -40.0 - 0.000 °C |
0.476 - 57.1 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 0.597 J/cm² Grade Count:136 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |