Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.40 - 1.90 J/cm² | 6.66 - 9.04 ft-lb/in² | Average value: 1.76 J/cm² Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.200 - 1.90 J/cm² @Temperature -40.0 - -20.0 °C |
0.952 - 9.04 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.924 J/cm² Grade Count:51 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact, Notched | 0.350 - 1.90 J/cm² @Temperature -40.0 - -30.0 °C |
1.67 - 9.04 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.784 J/cm² Grade Count:15 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 0.450 - 1.90 J/cm² @Temperature -30.0 - -30.0 °C |
2.14 - 9.04 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.16 J/cm² Grade Count:54 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.400 - 1.90 J/cm² @Temperature -30.0 - 30.0 °C |
1.90 - 9.04 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.870 J/cm² Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |