Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 - 0.700 J/cm² @Temperature 23.0 °C |
1.90 - 3.33 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eA |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Charpy Impact, Notched | 0.700 - 0.700 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.700 J/cm² Grade Count:1 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.350 - 0.700 J/cm² @Temperature -30.0 - -30.0 °C |
1.67 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.550 J/cm² Grade Count:10 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.700 - 0.700 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.700 J/cm² Grade Count:2 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.200 - 0.700 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 3.33 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.283 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Charpy Impact, Notched | 0.200 - 0.700 J/cm² | 0.952 - 3.33 ft-lb/in² | Average value: 0.529 J/cm² Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Charpy Impact, Notched | 0.500 - 0.700 J/cm² | 2.38 - 3.33 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact, Notched | 0.500 - 0.700 J/cm² @Temperature 23.0 °C |
2.38 - 3.33 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Charpy Impact, Notched | 0.600 - 0.700 J/cm² @Temperature -20.0 - -20.0 °C |
2.86 - 3.33 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.629 J/cm² Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 0.600 - 0.700 J/cm² @Temperature -20.0 - -20.0 °C |
2.86 - 3.33 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.680 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Charpy Impact, Notched | 0.200 - 0.700 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 3.33 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.445 J/cm² Grade Count:20 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Charpy Impact, Notched | 0.700 - 0.700 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.700 J/cm² Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.500 - 0.700 J/cm² | 2.38 - 3.33 ft-lb/in² | Average value: 0.600 J/cm² Grade Count:5 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact, Notched | 0.200 - 0.700 J/cm² @Temperature -40.0 - -20.0 °C |
0.952 - 3.33 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.391 J/cm² Grade Count:15 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.300 - 0.700 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.583 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Charpy Impact, Notched | 0.700 - 0.700 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.700 J/cm² Grade Count:1 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact, Notched | 0.400 - 0.700 J/cm² | 1.90 - 3.33 ft-lb/in² | Average value: 0.519 J/cm² Grade Count:7 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.100 - 0.700 J/cm² @Temperature -20.0 - -20.0 °C |
0.476 - 3.33 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.303 J/cm² Grade Count:11 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |