Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.60 J/cm² | 40.9 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Charpy Impact, Notched | 8.60 J/cm² | 40.9 ft-lb/in² | |
Arkema Group Kynar® FLEX 2800 PVDF