Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica PEEK Polyetheretherketone Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance w.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East) LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East) LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | |
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Styrolution Terblend® N NM-13 ABS/PA6 (Dry) Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ 200 15 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ 2060 15 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ 300 15 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Charpy Impact, Notched | 8.00 - 10.0 J/cm² | 38.1 - 47.6 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 BK431 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy PC/ABS polymer alloy general grade developed for automobile parts use. It has high heat resistance, impact strength, light resistance and fluidity, particularly, the high impact strength in a wide r.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | |
Akro-Plastic Akromid® A3 S1 PA, Cold-Impact Resistant
(discontinued **) The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
Unitika ET2025 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |
|||
Charpy Impact, Notched | 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo.. |