Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | ISO Data |
Styron Pulse® 710 ABS + Polycarbonate PULSE® 710 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 710 Engineering resin h.. |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | ISO 179 |
BASF Ultramid® B3Z BK 30464 PA6 (Dry) Description: Ultramid B3Z BK30464 is an impact-modified, pigmented black, unreinforced PA6 for injection molding.Applications: Impact-resistant articles, e.g. dowels.Information provided by BASF |
|||
Charpy Impact, Notched | 7.90 J/cm² | 37.6 ft-lb/in² | ISO 179/1eA |
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |