Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | ISO 179/1eU |
Lucite International Elvakon® 4470 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 6.40 J/cm² | 30.5 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |