Polymer Property : Charpy Impact, Notched = 5.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 5.60 J/cm²
26.7 ft-lb/in²
ISO Data
Styron Pulse® 1350 ABS + Polycarbonate
PULSE® 1350 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Charpy Impact, Notched 5.60 J/cm²
26.7 ft-lb/in²
ISO Data
Styron Pulse® 930 ABS + Polycarbonate
PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i..