Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 101R PC (Europe-Africa-Middle East) LEXAN 101R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 101R is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HP2R PC Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HP6REU PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® LI1813R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose PC having low levels of ionics species. UV-stabilized. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® ML104R PC (Europe-Africa-Middle East) LEXAN ML104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility inform.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 143 PC (Europe-Africa-Middle East) LEXAN 143 is a medium viscosity U.V. stabilized multi purpose grade. LEXAN 143 is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 950 PC (Europe-Africa-Middle East) LEXAN 950 is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HP4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | Injection Molded; ISO 179/1eA |
Styron DLGF9411.00 Polypropylene Overview: DLGF 9400.00 is a 40% long glass fiber reinforced grade with good flow properties. The glass fibers (12 mm length) are coupled to the polypropylene matrix resulting in high stiffness and s.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/1eA |
Borealis Daplen™ AK4504 TPO Compound Daplen AK4504 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen AK4504 is a material with excellent impact/stiffness ratio. Thanks to its low th.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 30.0 °C |
16.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 30.0 °C |
16.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 30.0 °C |
16.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 30.0 °C |
16.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 5051 (BGZ-40 FC) PA6-GF40 Product description: Grilon XE 5051 is a impact modified, heat stabilized PA 6 injection molding grade with 40% glass fiber reinforcement. Grilon XE 5051 has the following important properties: High.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 110 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | |
Akro-Plastic Akromid® B3 GF 30 S1 NAT. (1383) PA, Cold-Impact Resistant, 30% Glass Filled, Natural The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio.. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 144 PC (Europe-Africa-Middle East) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. |
|||
Charpy Impact, Notched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |