Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica PC Polycarbonate This amorphous polymer is commonly used for its high shock resistance even at low temperature. It is not a material recommended for mechanical applications, even if its dimensional stability does ma.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 S20 Nylon 6 for injection molding Nylon 6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: .. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179-1 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | |
Corbion Purac Blend C High Heat, Impact Modified Homopolymer PLA Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Increased impact is produced by addition of impact modifier to the base grade; a small am.. |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100T BK602 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T BK602 is a toughened high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where o.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |
|||
Charpy Impact, Notched | 2.30 J/cm² | 10.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |