Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | DIN 53453 |
Nilit RECONYL B S20 Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Ineos ABS Lustran® M201AS Increased chemical resistance compared to P2x, contains antistatic additives.,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179-1 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-3H PA12-GF30 Product description: Grilamid LV-3H is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-5H PA12-GF50 Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Arkema Group Rilsan® BMN P20 D Nylon 11 (Dry) Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL D720 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15 High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high glo.. |