Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Polimeri Europa Sinkral® B 532/E ABS Resin Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® E401 Very high surface resistance, high surface gloss.,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 50 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | |
Styrolution NOVODUR® P3H-AT ABS, Injection Grade Injection molding grade, antistatic, high gloss, improved chemical and dynamic resistance.Applications: Housings for telephones and household appliances. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 800 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO Data |
Styron Magnum™ 357HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179-1 |
Total HDPE 5502 R3 High Density Polyethylene - Blow Molding HDPE 5502 R3 is a high density polyethylene with good compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of blow molded pa.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30 Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW241F10 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 (2500) PA 6 Conditioned AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Conditioned, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179 |
BASF Ultramid® 1000-2 NF2001 PA66 (Conditioned) Ultramid 1000-2 NF2001 is a general purpose PA6/6. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFLEX P D72.1 Polyester-Elastomer, Shore D75 TPC-ETInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 30.0 °C |
7.61 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | |
BASF Luranyl® KR 2456/3 Polyphenylene Ether + Styrene-Butadiene Blend Heat resistant grade containing halogen-free flame-retardant. Mainly used for functional electronic parts that must meet tough fire-safety legislation.Data was collected by ISO methods and provided.. |
|||
Charpy Impact, Notched | 1.60 - 3.20 J/cm² | 7.61 - 15.2 ft-lb/in² | Average value: 2.22 J/cm² Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TRVX-50X9 black 9230 PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |
|||
Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | ISO 179 |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Dry) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |