Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | ISO 179/1eA |
Radici Radilon® AERV1906 LK (dry) Nylon 66 Glass-fiber reinforced with high impact strength, heat stabilizedInformation provided by Radici group. |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | ISO 179/1eA |
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI.. |
|||
Charpy Impact, Notched | 1.15 J/cm² @Temperature 23.0 °C |
5.47 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TV4 290 PBT-GF50 50% Glass Reinforced |
|||
Charpy Impact, Notched | 1.15 J/cm² @Temperature 30.0 °C |
5.47 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | |
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi.. |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | ISO 179 |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | ISO 179 |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | |
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold... |
|||
Charpy Impact, Notched | 1.15 J/cm² @Temperature -30.0 °C |
5.47 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 1.15 J/cm² | 5.47 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast. |