Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |
|||
Charpy Impact, Notched | 0.750 J/cm² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179 |
GEHR Plastics POM-ELS Acetal, Electrically Conductive Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene G2855 High Density Polyethylene CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
LATI Latishield 66-08A G/25-V0KB1 PA66, Steel/Glass Fiber Reinforced, Flame Retardant EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
LATI Latistat 67-08 PA66, Impact Modified Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: .. |
|||
Charpy Impact, Notched | 0.750 J/cm² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® AV2 370 XL-T PET-GF35 35% Glass Reinforced, Low Outgassing, Thermal conductive material |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced PEEK-GF30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBATER BFA15 PBT, 15% glass fiber reinforced, flame retardant PBT-GF15 FRInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
Cathay PA512 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Charpy Impact, Notched | 0.750 J/cm² @Temperature -30.0 °C |
3.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 683 Polypropylene Copolymer Copper ResistantInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl PMD 20117 Flame Retardant Nylon, Glass Filled Flame retardant, glass fiver reinforced, friction resistantInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I.. |
|||
Charpy Impact, Notched | 0.750 - 0.750 J/cm² @Temperature -30.0 - -30.0 °C |
3.57 - 3.57 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.750 J/cm² Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |