Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.640 J/cm² @Temperature 23.0 °C |
3.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.640 J/cm² @Temperature -30.0 °C |
3.05 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.640 J/cm² | 3.05 ft-lb/in² | ISO Data |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Charpy Impact, Notched | 0.640 J/cm² @Temperature 23.0 °C |
3.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG20-DN00N1 Nylon 6 20% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 0.640 J/cm² @Temperature -30.0 °C |
3.05 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.640 J/cm² @Temperature 23.0 °C |
3.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TV4 244 S PBT-GF20 FR 20% Glass Reinforced, Flame Retardant |
|||
Charpy Impact, Notched | 0.640 J/cm² | 3.05 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6 15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resista.. |
|||
Charpy Impact, Notched | 0.640 J/cm² @Temperature -30.0 °C |
3.05 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i.. |
|||
Charpy Impact, Notched | 0.640 J/cm² | 3.05 ft-lb/in² | ISO 179 |
BASF Ultradur S 4090 G4 BK5110 20% Glass Filled PBT Ultradur S 4090 G4 BK5110 is a 20% glass reinforced, pigmented black PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkag.. |
|||
Charpy Impact, Notched | 0.640 J/cm² | 3.05 ft-lb/in² | ISO 179 |
BASF Nypel® 6030G HS DB BK 5830 30% Glass Filled PA6 (Dry) Description: Nypel® 6030G HS DB BK5830 is a 30% glass fiber reinforced, heat stabilized, black pigmented, injection molding compound based on recycled PA6..Application: Nypel® 6030G HS DB BK5830.. |
|||
Charpy Impact, Notched | 0.640 J/cm² | 3.05 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® GH-25D Acetal Co-polymer (POM), GF 25% reinforced, High flow, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |