Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.560 J/cm² | 2.66 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.560 J/cm² | 2.67 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.560 J/cm² | 2.67 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.560 J/cm² | 2.66 ft-lb/in² | ISO 179 |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.560 J/cm² | 2.67 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® C5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.560 J/cm² @Temperature 23.0 °C |
2.66 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact, Notched | 0.560 J/cm² | 2.67 ft-lb/in² | |
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |