Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Tepcon M270 Acetal-copolymer (POM), High Fluidity, High Cycle Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | GB-1043 |
Zhejiang Juner PA-A6-3 GF/MF Reinforced Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 711SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® M270-44/M270S Acetal Co-polymer (POM), Standard, High flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.530 - 0.600 J/cm² @Temperature -40.0 - -30.0 °C |
2.52 - 2.86 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.560 J/cm² Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® M270-45 Acetal Co-polymer (POM), Weather resistance, High flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.530 J/cm² | 2.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® M270-48 Acetal Co-polymer (POM), Antistatic, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |