Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.460 J/cm² @Temperature -30.0 °C |
2.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.460 J/cm² | 2.19 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature 23.0 °C |
2.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature 23.0 °C |
2.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG15-DN00N1 Nylon 6 16% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 0.460 J/cm² | 2.19 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 2016 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50% DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.460 J/cm² | 2.19 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 751SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.460 J/cm² | 2.19 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -30.0 °C |
2.19 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -30.0 °C |
2.19 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -30.0 °C |
2.19 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |