Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A12^ F25 NH10 Nylon 66, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179/1eA |
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Charpy Impact, Notched | 0.450 J/cm² - NB @Temperature -40.0 - -30.0 °C |
2.14 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
Average value: 5.40 J/cm² Grade Count:46 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**) Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2346S Polypropylene Block Copolymer CHARACTERISTICS: HIGH STIFFNESS, HIGH FLOW, GOOD IMPACT, HEAT STABILITY CONTAIN ANTISTATIC AND UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® C1S25 PA6/PA66 Blend, Unreinforced Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179 |
Total PPH 7060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7060 is homopolymer.ApplicationATOFINA Polypropylene PPH 7060 is intended for the injection molding of packaging containers, toys, domestic appliances, garden furniture and.. |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® S600F40 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 BK851 is an unreinforced lubricated low viscosity black polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS LC3030 NC010 Nylon 610
(Unverified Data**) Zytel® RS LC3030 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, low viscosity grade, developed for extrusion a.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPHC K8030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 - 0.600 J/cm² | 2.14 - 2.86 ft-lb/in² | Average value: 0.550 J/cm² Grade Count:3 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2340S Polypropylene Block Copolymer CHARACTERISTICS: HIGH FLOW, HIGH STIFFNESS, HEAT STABILITY, GOOD IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, THIN WALL PARTS |
|||
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |