Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.390 - 0.500 J/cm² @Temperature -30.0 - -20.0 °C |
1.86 - 2.38 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.430 J/cm² Grade Count:3 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST25G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ISO 179/1eA |
Lucite International Elvakon® 4474 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ASTM D256 |
Plenco 6401 Phenolic, Briquette, Injection Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 7195W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | |
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | |
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.390 J/cm² @Temperature -30.0 °C |
1.86 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
Charpy Impact, Notched | 0.390 J/cm² | 1.86 ft-lb/in² | ISO 179 |
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 BKQ642 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |
|||
Charpy Impact, Notched | 0.390 J/cm² @Temperature -30.0 °C |
1.86 ft-lb/in² @Temperature -22.0 °F |
ISO data |
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen.. |
|||
Charpy Impact, Notched | 0.390 - 8.00 J/cm² | 1.86 - 38.1 ft-lb/in² | Average value: 0.991 J/cm² Grade Count:23 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |