Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.360 J/cm² @Temperature 23.0 °C |
1.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179 |
PolyOne Bergamid™ A70 G5 T Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature -30.0 °C |
1.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)
(Unverified Data**) Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f.. |
|||
Charpy Impact, Notched | 0.360 - 1.20 J/cm² | 1.71 - 5.71 ft-lb/in² | Average value: 0.866 J/cm² Grade Count:10 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Charpy Impact, Notched | 0.360 - 4.00 J/cm² | 1.71 - 19.0 ft-lb/in² | Average value: 1.37 J/cm² Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature 23.0 °C |
1.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 8540 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature 23.0 °C |
1.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Terralene® WF 6534 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla.. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature -20.0 °C |
1.71 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® C7640 Polybutylene Terephthalate (PBT), Super low warpage, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature -30.0 °C |
1.71 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature -30.0 °C |
1.71 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Appryl® CZN 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for interior trim applications, that required an excellent impact test associated with a high modul.. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature -30.0 °C |
1.71 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I.. |
|||
Charpy Impact, Notched | 0.360 J/cm² @Temperature -30.0 °C |
1.71 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Appryl® CZU 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for exterior trim automotive applications, that required an excellent impact test associated with a.. |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179 |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.360 J/cm² | 1.71 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® GM-20 Acetal Co-polymer (POM), Low warpage, GF 20% reinforced DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |