Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 648 MPa @Temperature 25.0 °C |
94000 psi @Temperature 77.0 °F |
0°, Wet, Fill Compression |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 648 MPa @Temperature 24.0 °C |
94000 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Compressive Yield Strength | 648 MPa @Thickness 25.4 mm |
94000 psi @Thickness 1.00 in |
LT Direction |
Alcoa 7055-T77511 Aluminum Extrusions Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |