Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 607 MPa @Temperature 82.2 °C |
88000 psi @Temperature 180 °F |
0°, Wet, Fill Compression |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |