Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0510 MPa @Strain 25.0 % |
7.40 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.0510 MPa @Strain 25.0 % |
7.40 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.0510 MPa @Strain 25.0 % |
7.40 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.0510 MPa @Strain 10.0 % |
7.40 psi @Strain 10.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.0510 MPa @Strain 10.0 % |
7.40 psi @Strain 10.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.0510 MPa @Strain 40.0 % |
7.40 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi.. |
|||
Compressive Yield Strength | 0.0510 MPa @Strain 25.0 % |
7.40 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 302/T-E NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |