Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0270 MPa @Strain 25.0 % |
3.92 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi.. |