Polymer Property : Compressive Yield Strength = 12500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 86.0 MPa

@Strain 2.00 %
12500 psi

@Strain 2.00 %
dry; ISO 604
Murtfeldt Murpec® SP Polyetheretherketone
Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• ..