Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0820 MPa @Strain 40.0 % |
11.9 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.0820 MPa @Strain 40.0 % |
11.9 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.0820 MPa @Strain 50.0 % |
11.9 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam VUL 401 Polyurethane Foam Used for the production of springs and shock-absorbing details in the automobile industry, seals for trunks and joints for ball bearings, pressure barsInformation provided by Eurofoam s.r.l. |